Zinc vs Aluminium Die Castings for Hardware Parts

Author: Technical TeamReviewed by: Tooling EngineerPublished: 1 November 2026Updated: 1 November 20269 min read

QUICK ANSWER

Aluminium alloy is chosen for larger, lighter parts where weight and corrosion behaviour matter. Zinc alloy is chosen for small parts with thin walls, fine detail and internal threads. Both are die cast in the same plant, so the choice is driven by the part, not by which process is available.

Two alloys, one process family

Both materials are cast in a steel mould under pressure, then trimmed, machined and finished. The equipment is similar, but the way each alloy fills a cavity and cools is not.

Aluminium alloy is lighter and is usually specified where the part is large, handled often or shipped in volume. It needs a finish that suits its own surface chemistry. Its lower density also changes how the carton is built.

Zinc alloy is denser and casts fine shapes with less trouble at thin sections. That is why small connectors, brackets and inserts often come in zinc.

How the two materials behave on a part

Zinc fills thin walls and sharp corners more readily, so a small part keeps its detail without heavy draft. The trade-off is weight and, in some designs, a heavier feel in the hand.

Aluminium is lighter and suits longer shapes, but thin sections and fine internal threads need more thought. Where a thread must carry load repeatedly, a design review usually decides the fix.

Both alloys are cast to the drawing, and machined features are held to ±0.5 mm. Material choice does not change that rule, but it does change how much machining a part needs.

Where aluminium suits furniture and rack hardware

Shelf supports, long brackets and visible frame parts benefit from lower weight. On a display rack that is moved between shows, that difference is felt every time it is packed.

Aluminium also takes anodising, which keeps a metallic look without a paint film. That suits fittings where the surface is the design, not only the protection.

The usual limit is size, not strength. Very small parts with internal threads are often better in zinc, even when the rest of the assembly is aluminium.

Where zinc suits small precise hardware

Tube connectors, sofa feet inserts, small hinges and corner brackets are typical. These parts are small, need accurate bores and often carry a screw thread that runs through the casting.

Zinc also casts crisp edges, which matters where the part is seen at close range, such as a foot or a handle end. Visible detail is cheaper to cast than to machine.

The usual limit here is weight and size. A large visible panel in zinc would add kilos to a piece of furniture and change how it is handled in the shop.

Surface finishing on each material

Zinc takes plating and painting well, and polished zinc can be made to look like brass or chrome. Pre-treatment decides whether the coating holds on an edge, not the colour alone.

Aluminium is usually anodised, powder-coated or painted. Anodising is a conversion of the surface itself, so it does not chip like a film, but colour ranges are narrower.

Salt spray testing to ISO 9227 is available on request, with the duration agreed on the drawing. We do not publish a single figure that applies to every part.

Tooling and cost drivers

A new mould takes about 25 days from drawing approval, whichever alloy is used. The difference sits in cycle time, material price and how much machining the part needs afterwards.

Comparing a zinc and an aluminium design by price per kilogram rarely helps. Compare the finished part at the same quantity, including machining, finishing and packing.

If the part already exists in one material, ask what changes if it moves to the other. Sometimes the mould stays similar and only the walls change, and sometimes the whole design has to follow.

What the A and X prefixes tell you

In our catalogue, a part number starting with A is a die-cast aluminium alloy part, and one starting with X is a die-cast zinc alloy part. Original mould numbers beginning with P, M or B use either alloy.

The prefix is a quick pointer, not a specification. Always confirm the alloy on the drawing, because a part number can stay the same while the material changes for a customer run.

When a part is quoted, the alloy is written in the offer. If your drawing names a grade we do not run, we say so before the tooling stage rather than after.

Deciding with a drawing and a sample

Send the drawing, the quantity and where the part will be used. Our tooling engineers review it within three days and note any point where the material choice creates risk.

Samples come seven days after drawing approval, in the alloy quoted. Handle them next to the parts you use now, because weight and edge feel rarely survive a data sheet.

If both alloys are possible, we can quote both so the decision is made on cost and feel together. That is usually faster than settling the material before the first drawing exists.

Matching the alloy to the finish you already run

If you already run a plating or powder line, the alloy has to suit it. A part that looks right on a sample can fail on your line because the pre-treatment differs from ours.

Colour matching across two alloys is harder than within one. Where visible parts of an assembly meet, keeping a single alloy usually saves a colour argument later.

Send a reference part in the finish you want to match, and say which areas must stay free of coating. Masking threads and bores is decided on the drawing, not on the line.

Questions to settle before tooling starts

Wall section, draft and thread depth come first, because they decide whether the part casts cleanly in the chosen alloy. A drawing that ignores them returns a list of questions and a delayed start.

Then the finish: colour reference, gloss level and salt spray duration if you test. Anything still open stays TBC in the offer, so nothing is assumed on your behalf.

Finally packing and inspection. AQL 1.0 covers the outgoing check, and the carton, label and pallet pattern are agreed with the first shipment so repeat orders arrive the same way.

  • Alloy, wall section, draft and thread depth on the drawing.
  • Colour reference, gloss and salt spray duration if tested.
  • Packing, label and inspection level for the first shipment.

Questions from Buyers

It depends on the alloy and the section, not on the family name. For a small threaded part zinc usually performs better, while for a large light bracket aluminium is often the practical answer.

Send Your Drawing, Get a Written Quote in 24 Hours

A drawing, a sample or a target price is enough to start. Tooling in 25 days, samples in 7 days.

Email your drawing
鄂ICP备2026043223号-1