Keeping Colour Consistent Between Production Batches
QUICK ANSWER
Colour drifts when the sample, the lighting or the bath chemistry changes. Hold one approved physical sample per colour, state the viewing light on the drawing, and check the first articles of every run. Outgoing lots are inspected at AQL 1.0 against that sample.
Why batches drift
Plating bath chemistry, powder lot and oven temperature all move slightly over time. Each shift alone is small, but two shifts together can be visible on a shelf line.
The same part also looks different under daylight, warm shop light and a phone screen. That is why a verbal colour name is a weak specification.
One approved sample per colour
Approve a physical sample from the first run and keep it with the drawing. Later orders are matched to that piece, not to a photograph.
For frames with several parts, approve them together as one set. A connector matched on its own may look wrong once assembled on the tube.
Control the line, not only the final check
The first articles of every run are compared with the approved sample before the rest of the lot is finished. If the match is out, the bath or powder is adjusted first.
Records of the check stay with the lot, so a question months later can be traced to a run rather than to a general claim.
What to write on the purchase order
Name the sample reference, the finish type and the viewing condition. If a colour tolerance is critical, state how the match will be judged.
Anything not stated stays TBC and is confirmed in the quotation. We do not assume a colour standard that has not been agreed in writing.
Questions from Buyers
Small shifts in bath chemistry, powder lot or oven temperature add up. A physical sample per colour, kept from the first run, makes the difference visible early.
Send Your Drawing, Get a Written Quote in 24 Hours
A drawing, a sample or a target price is enough to start. Tooling in 25 days, samples in 7 days.